3. Sanding

Sand the surface evenly, particularly at the area where the PP material and putty meet.

Use a flexible block and #240~#400~#600 sandpaper.

4. Air blowing / degreasing

Use alcohol, a tack cloth, and wax and grease remover.

5. Spraying primer surfacer

NOTE:  Spray the bumper primer on the area where the PP material was exposed and around the putty.

-

Spray the primer surface wider then the putty and painted surfaces of bumper primer.

-

Spray 2 to 3 coats to get 20 to 30 microns of thickness.
-

Use the 2-component type primer surfacer (gray) and a spray gun.

-

Follow the materials manufacturer's instructions.

Drying

NOTE: Take care not to let the heat lamp deform the bumper during the drying process.

6. Sanding

After drying, wet sand the area of the intermediate coat.

Use the #600 sandpaper.

NOTE:  Do not use #600 or less.

7. Air blowing /degreasing