Hombre XS Space Cab 2WD V6-4.3L (1998)
softening of the races or the rollers. In order to check for loss of temper on the races and the rollers, perform a file test. A file drawn over a tempered part
will grab and cut the metal. A file drawn over a hard part will glide readily with no metal cutting. Replace the bearings if overheating damage is
indicated. Check the seals and the other related parts.
MISALIGNMENT
The outer race is misaligned due to a foreign object. Clean the related parts. Replace the bearing. Ensure the races are properly sealed.
CRACKED INNER RACE
A cracked race may be due to improper fit, cocking, or poor bearing seats. Replace the bearing. Correct the bearing seats.
FATIGUE SPALLING
Spalling is a flaked surface metal that results from fatigue. Replace the bearing. Clean all related parts.
BRINELLING