Test result evaluation for the battery testing at discharge status |
Due to the intense discharge to which the battery is submitted during this test the battery voltage will fall. |
t
| If a battery is in working order battery voltage will only drop to lowest voltage. |
t
| If the battery is defective or has a low charge, the battery voltage quickly drops below the minimum voltage. |
t
| After the test, this low voltage value remains for a long period, and the voltage only rises slowly. |
t
| Carry out the test once only. Repeating the test will cause a false measurement. |
t
| To test another battery (one more) the tester should cool during some 30 minutes, with the aim of obtaining a correct result in the measurement. |
|
|
|