Body - Paint Chipping On Rear Quarter Panel|Page 4178 > < Body - Paint Chipping On Rear Quarter Panel|Page 4176
Page 6
background image

Caution:

Do not hit the panel clinched area; this could cause the paint to crack.

Note:

Inspect paint, repair as necessary following the procedure listed in the introduction of this bulletin.

Note:

Paint repairs must be completed prior to installation of the new protective film.

Note:

Allow at least 48 hours for paint to dry before installing film.

Note:

If film replacement is required on one side, both sides must be replaced at the same time.

Protective film (3 pieces) taped into place for illustration purposes.

Remove the old film. Using mild detergent mixed with water, clean the area that will be covered with the new film. Clean a second time using rubbing
alcohol.

Note:

Vehicle and film must be at room temperature for proper adhesion. Do not install protector film dry. There are 3 pieces that need to be installed. The
following steps need to be repeated for each piece installed.

Spray the area where the protective film will be installed with mild detergent mixed with water.

The protector film consists of 3 layers, white backing, protector film and template.

Body - Paint Chipping On Rear Quarter Panel|Page 4178 > < Body - Paint Chipping On Rear Quarter Panel|Page 4176