- Read measured value on hydrometer and compare with table:

Electrolyte density must be at least 1.24kg/dm3.

- Charge battery if density is insufficient.

- Repeat density check after charging battery.

Measured value for electrolyte density of individual battery cells must not differentiate more than 0.03 kg/dm3.

Example of unacceptable deviations in electrolyte density:

Example 1:  The electrolyte density in cell 4 is too low.

Example 2:  The electrolyte density in cells 4 and 5 is too low. The electrolyte density deviations between the battery cells is more than 0.03 kg/dm3

- If the specifications are not obtained, replace battery.

- If the specifications are obtained, screw plugs in again.

It is absolutely necessary to use original sealing plugs in the battery screwed openings to guarantee the battery is sealed correctly.

Use original sealing plugs of same construction if lost or damaged.

The sealing plugs must be installed with an 0- ring.

Visual Check

Visual check

Carry out a visual check of the battery before performing measurements such as no load voltage, electrolyte specific gravities or battery load test.

Notes: Performing this test establishes:

- Whether the battery housing is damaged. Electrolyte can leak out if the housing is damaged.

- Whether the battery terminals (battery wire connections) are damaged. Wiring connector contact cannot be guaranteed if the battery terminal is
damaged. This may cause a cable to spark or burn, which may cause malfunctions in the electrical system.