Tape the front side of the damage with 3M 6945 masking tape
Use 3M 5900 or 3M 5895 Flexibel Part Repair Material. Mix parts A and B equally, to an even color.
Application should be carried out within 5-6 minutes.
Alternatively the reinforcement material of fiberglass weave, aluminum or plastic can be used. If plastic is used the plastic should be the same type as the
damaged material.

Fix the damaged area 
Wet the surface with a thin layer of 3M 5900 using a putty knife. If the damage has gone through the bodywork plastic should be pressed against the
masking tape.
if necessary reinforce by laying 2 to 4 layers of fiberglass weave (close knit) crosswise
Allow to cure for 20-30 minutes at room temperature (20°C (68°F)).
After curing remove masking tape on the front.

Fine sand the area 
Sand the area with P180 sandpaper.
If there are pores or sanding scratches first spray a thin layer of 3M 5907 PAP and allow to dry.
Then fill with a thin layer of 3M 5903.
Fine sand with P 600 sandpaper.
Spray a thin layer of 3M 5907 PAP and allow to dry.
Then spray a mist coat and two spray coats of 3M 5906 Flexibel Parts Coating over the repair area and the surrounding area.
Allow to dry approximately 30 minutes.
If necessary sand lightly with Scotch-Brite finark gray 7448 or 3M 622 Frecut P500.

Plastic Repairs With Teroson

Plastic repairs with Teroson 

Clean plastic component 
Clean plastic component thoroughly with soap and water. Dry it.
If necessary align the component to the original (tension free) shape using hot air.
Note the risk of overheating.

Clean the damaged area 
Clean the damaged area on both in- and outsides with Cleaner FL.
Air 15-20 minutes.

Sand the damaged area 

Sand damaged area to a wedge shape (1-2 cm). Use sandpaper P120.
If the damage is a crack, drill a hole (approximately 2 mm in diameter) at the end of the crack. Widen the damaged area mechanical (to approximately
1-2 mm) and then sand.
Roughen the damaged on both sides for better adhesion.

Repeat cleaning process 
Repeat cleaning process on the damaged area on the in- and outside with Cleaner FL
Air 15-20 minutes.

Spray Terokal-150 