Base filler designed for surfaces which are not as uneven as for coarse base filler.  Mix carefully with the accompanying hardener. Refer to the
instructions on the can.
All the necessary base filler data is found in the specifications, see  Application data for paint materials See: Application and ID.

Allow the base filler to dry. 
The data given below is approximate and can vary for different manufacturers. Therefore always follow the manufacturers' recommendations.
Drying time 20-30 min at room temperature (20°C).
Accelerated drying can be used on the base filler as follows:

Note! There is always a risk of paint work cracking with the accelerated drying of polyester products. 

Sand the base filler with dry sandpaper P 180 and an oscillating sanding machine. 