CL TYPE S V6-3.2L SOHC (2001)
Paint: Service and Repair
Preprocessing of Painting
Preprocessing of Painting
1. Featheredging
NOTE:
-
The paint film damaged area should be sanded flat and smooth.
-
If this is not done correctly, the end results will not be acceptable.
Damage to metal surface:
-
Sand the damaged area flat and smooth.
Use a disc sander and #60-#80 disc sandpaper
Use the double action sander and #60#80 disc paper.
-
Sand the area larger than the damaged area.
Use a double action sander and #180-#240 disc sandpaper.
-
If a double action sander is not available, use a rubber pad and wet or dry sandpaper.
Use a flexible block and #280, #340, #400, #600 sandpaper.
Damage to undercoat, intermediate coat and top coat:
Sand the damage area flat and smooth