RSX L4-2.0L (2005)
Paint: Service and Repair
Preprocessing of Painting
Preprocessing of Painting
1. Featheredging
NOTE:
-
The paint film damaged area should be sanded flat and smooth.
-
If this is not done correctly the end results will not be acceptable.
Damage to metal surface:
-
Sand the damaged area flat and smooth.
Use the disc sander and #60-#80 disc paper.
Use the double action sander and #60-#80 disc paper.
-
Sand the area larger than the damaged area.
Use the double action sander and #180-#240 disc paper.
-
If a double action sander is not available, use a rubber pad and wet or dry sandpaper.
Use the flexible block and #280, #340, #400, #600 sandpaper.
Damage to undercoat, intermediate coat and top coat: Sand the damage area flat and smooth