Repairing slight damage on rims |
WARNING t
| Repairing a damaged wheel rim or disc by heating, welding or adding or removing material is strictly prohibited. |
t
| Damaged or deformed rims and rims with cracked or deformed bolt holes must not be repaired. |
t
| Rims can only be repaired with approved and specified Genuine Paintwork material. |
t
| After rims have been repaired, the manufacturer will no longer accept any warranty claims. |
|
Rims with cracks at the edges must not be repaired; they must be renewed immediately. |
Any form of cutting/machining, heating and welding is not permissible. |
Straightening of deformed material is not permissible. |
The radial and axial runout must not exceed the production tolerance of 0.8 mm prior to repair. |
Only cast light alloy wheels may be repaired using filler compound. These wheels are marked on the inside with the material designation AlSi xx. |
Forged wheels may only be painted. |
Repairing damage is limited to painted surfaces. |
Bright-turned rims with only one coating of clear varnish must not be repaired. |
It is only permissible to repair damaged surfaces on the visible side of the wheel (decorative outside surface). |
Damage that is deeper than 1 mm must not be repaired. |
Do not fill in material closer than 50 mm from outer wheel flange. |
|
|
|