Shallow Scratch:
Use a flexible block and #240 - #400 - #600 sandpaper.

Hole/Deep Gouge:
Cut out and make any torn or burred area flat.
Use a knife, flexible block, and #180 - #240 sandpapers.

2. Air blowing/degreasing

Clean the damaged area throughly.
Use alcohol, and wax and grease remover.

Undercoating

Undercoating 

1. Spraying primer Primer is used to fill cavities in the putty and primer surfacer.

-

Spray primer on the exposed area. 

-

Spray the 2 - 3 coats of primer on 2 - 3 coats over the area you applied puny. 

-

Apply primer to the back of the bumper if the damage is a tear or hole.

-

Bumper primer

-

Warm the primer if the ambient temperature is below 50 degrees F (10 degrees C).

-

Follow the bumper primer manufacturer's instructions.

-

Use a spray gun and a brush.

Drying 

NOTE: Take care not to let the heat lamp deform the bumper during the drying process.

Dry the bumper primer thoroughly with an infrared dryer or other suitable method.

Drying Time: