Use the double action sander and #60-#80 disc paper.
-
Sand the area larger than the damaged area.
Use the double action sander and #180- #240 disc paper.
-
If a double action sander is not available use a rubber pad and wet or dry sandpaper
Use the flexible and #280,#340,#400,#600 sandpaper.
Damage to undercoat, intermediate coat and top coat
Sand the damage area flat and smooth
Use the double action sander and #180-#240-#320 disc paper.
2. Preparing metal surfaces.
Remove all corrosion from the damage area.
Use a product that removes.
3. Air blowing/degreasing
Use alcohol, wax, and grease remover.
Treatment of Metal Surface
Treatment of Metal Surface
1. Filling/drying
Small cracks or pinholes in the sheet metal should be repaired with a body filler and sanded flat and smooth.
-
Use the 2- part polyester resin putty.
-
Mix the putty with the hardener in the correct ratio.
-
Follow the body filler manufacturer's instructions.
-
Mix the body filler and hardener quickly.
-
Apply the body filler in several thin coats, without air bubbles.
-
Do not try to cover the surface with one heavy coat.