Worn surface. Advanced wear has led to a situation where only the remains of the original surface are left.

It is clear that the roughness is caused not only by depressions but also by bumps.

Replace brake discs! To do this, follow the instructions.

In general, the following applies: Brake discs must be replaced if the surface roughness (Rk) is > 80 microns!

3. Worn brake discs (special cases):

PCCB surface roughness (Rk) = 108 micrometers

3.1.

Surface roughness Rk = 108 microns, as for previous disc, but with some of the original friction surface remaining -arrow-.

Replace brake discs! To do this, follow the instructions.

In general, the following applies: Brake discs must be replaced if the surface roughness (Rk) is > 80 microns!

PCCB brake disc

3.2.

Surface roughness (Rk) = 72 microns. Borderline brake disc detected based on roughness, as well as wear indication and connected surface
fractures -arrows-, > 1 cm2.

Replace brake discs! To do this, follow the instructions.

Checking minimum thickness of brake discs

Information

Minimum thickness of PCCB brake disc