7. Place the component in a varnishing furnace set to 60 degrees C so that the structure hardens.

Tip: The mixture can also be used to raise very small plastic burrs on ground surfaces. Afterwards, harden the component in an oven at 60 degrees
C and rub down with Scotchbrite or similar.