Drill out original joint using spot weld breaker.

Drill out original joint using spot weld breaker.
Part section repair is possible using separating cut (a).

Remove remaining material using compact angle grinder.

- Upper inner longitudinal member
- Upper longitudinal member
Grind welding surfaces down to bright metal.
Prepare flanges on new part for welding.
Drill holes for SG plug weld seam, 8 mm ∅ using drill.

Note
- Due to the different types of steel and panel thicknesses employed, one of the welding units (inverters) listed under "Tools" must be used to ensure correct results when spot welding.
Weld in upper inner longitudinal member at suspension turret using resistance spot welder: RP spot weld seam.
Weld in at separating cut using shielded arc welding equipment: SG continuous seam.

Weld in upper inner longitudinal member using shielded arc welding equipment: SG plug weld seam.
Weld in upper longitudinal member for wheel housing using resistance spot welder: RP spot weld seam.

Parts & tools for this job For 2008 Audi A3
- PARTClutch kitSearch: Audi A3 2008 clutch kit
- TOOLClutch alignment toolSearch: clutch alignment tool
- FLUIDGear oilSearch: Audi A3 manual gearbox oil
As an Amazon Associate we earn from qualifying purchases.