C70 L5-2.4L Turbo VIN 63 B5244T7 (2003)
This is the way the original paint is applied in the factory (see illustration). For the best finish, quality and durability.
A Panel
B Phosphatizing
C Ed
D Stone chip paint (front edge of hood)
E Filler
F Base solid or Base metallic
G Varnish
Sand-Blasting
Sand-Blasting
All corrosion products on the panel must be removed before painting. Sand-blasting is a very effective method of doing this, particularly for deep rust
damage.