Page 31
background image

 Only spray one part varnish on the surrounding area (B).
Directly afterwards spray pearl in approximately 2 spray coats. The number of spray coats depends on the result of the test painting.
The first coat is sprayed on a smaller area (C), approximately 10 cm around the damaged area. The following coat is sprayed on the surrounding area
(B). Each coat increases the sprayed area around the damaged area a little.

Air between coats 
 Air at room temperature (20°C (68°F)) for approximately 15 minutes between coats.
 Only spray a thin coat of one part varnish on the surrounding area, to retain the flow of the pearl coat.
If necessary spray a pearl coat on a smaller area (C), approximately 10 cm around the damaged area and on the surrounding surfaces (B), directly
afterwards. Color powder from the pearl paint is absorbed by the one part varnish coat.
 Air for approximately 30 minutes at room temperature (20°C (68°F)) before final spraying with two part varnish.

Paint with two part varnish 
Paint the damaged area and the surrounding area with two part varnish.

Finishing

Finishing 

General about finishing 
Polishing can in many cases avoid the need to repaint. As a rule small faults like scratches, dirt, spray mist etc can corrected by machine polishing.

Remove any surface defects 