Use fine base filler to even out any small hollows and recesses remaining visible after applying the primer. The base filler is applied in thin layers, max 3
layers per hour.
 Allow the base filler to dry and sand down the fine base filler using P 320 sandpaper. 
Spray on the primer.

Wet sand the surface on which the primer has been applied using P 600 sandpaper. 