01 4-cylinder direct injection engine (1.8 ltr., 2.0 ltr. 4V TFSI, generation II)02 Fuel supply system, petrol engines03 4-cylinder direct injection engine (1.4 ltr. 4-valve TFSI EA 211)04 4-cylinder direct injection engine (1.8 ltr., 2.0 ltr. 4V TFSI, generation III)05 4-cylinder TDI engine (2.0 ltr. 4-valve common rail EA 189 - generation II)06 Fuel supply system, diesel engines07 5-cylinder direct injection engine (2.5 ltr. 4-valve TFSI)08 4-cylinder TDI engine, 2.0 ltr. 4-valve common rail (EA 288 Gen. I)09 Technical data for engines10 Rear final drive 0AY, 0BR, 0BS, 0CR11 Servicing 6-speed manual gearbox 02Q, 0BB, 0FB12 7-speed dual clutch gearbox 0BH (S tronic)13 6-speed manual gearbox 02Q, 0BB14 6-speed manual gearbox 0A615 6-speed dual clutch gearbox 02E16 Running gear: Specifications for testing the braking force (according to German legislation)17 Running gear: Trailer Operation Guide18 Running gear, axles, steering19 Brake system20 Running gear: Wheel/Tyre Guide21 Heating, air conditioning22 Electrical system23 Electrical: Communication24 General body repairs, exterior25 General body repairs, interior
Audi Q3 8U (2011-2018)11 · Servicing 6-speed manual gearbox 02Q, 0BB, 0FB
11 · Transmission

Dent removal

Make
Audi
Model
Q3 8U
Year
2011–2018
Section
Bevel box › Dent removal
Servicing 6-speed manual gearbox 02Q, 0BB, 0FBDent removal

Dent removal

AudiBinderBody repairsAudi TT2015Edition01.2015

The danger of over-stretching the material is greater with aluminium than with steel.

Sharp-edged or hard panel beating tools (e.g. steel hammer) should not be used. Use plastic, wood or aluminium hammers instead.

Direct panel beating procedures, i.e. aluminium panel is positioned directly between counter-hold tool and panel beating hammer, should be kept to a minimum.

Unlike the procedure for steel panels, you should begin in the middle of the dent when removing dents on aluminium panels.

Where possible, aluminium panels should be pressed rather than beaten.

When finishing the metal (planishing), the dolly (support tool) should be held loosely. If you apply excessive force when finishing you could stretch the material. For this reason you should use a support tool made of hardwood.

If material stretching should occur, it can be eliminated by heating and shrinking.

Warning Heat shrinkage temperature max. 150° C.

Warning If a crack or rupture appears during panel beating, the part must be renewed!