7.  Allow primer to dry as follows:

^  285-50 - For 3 hours at 68°F
^  285-95 - For 4 hours at 68°F

or force dry for 40 minutes at 120°F

8.  Wet sand primer after drying time with 400/600 (P800-P1200) grit paper.

9.  Wet sand entire area to be painted with 400/600 (P800-P1200) grit paper

PAINTING PROCEDURE

NOTE: Ten percent base coat activator (355-55) should be added to the base coat to ensure maximum stone chip resistance.

1.  Mix base coat as follows:

^  100 parts by volume of base coat 55 Line
^  40 parts by volume of reducer 352-50,91
^  10 parts by volume of 355-55

2.  Apply two coats of 55 Line" base coat to the entire area allowing three to five minutes between coats.

3.  Allow basecoat to flash 10 minutes or until matte.

CAUTION: Elastifier must be added to clear coat before hardener.

4.  Elastify clear coat 25% by volume (4:1 ratio)

5.  Apply 2 coats of elastified clear coat allowing two to three minutes flash between coats.

CAUTION: Plastic parts can deform during baking if not supported properly. If parts are removed from the vehicle use a lower force dry
temperature (120°F for 40 minutes)

6.  Force dry at 140°F for 30 minutes.

CAUTION: Allow 24 hours drying time before attempting to polish to remove dirt nibs or similar imperfections.

7.  Polish surface as required after 24 hour drying time.