01 Technical Data02 Self diagnosis, V.A.G Inspection Service03 Engine assy, cylinder block, crankcase04 Enginecrankshaft group, pistons05 Engine cylinder head, valve gear06 Engine lubrication07 Engine cooling08 Fuel supply, gas operation09 Mixture preparation system, electronic inj., Gas10 Exhaust system11 Starter-current supply-CC12 Ignition system, glow plug system13 Clutch, control14 Gearbox mechanics, operation, construction, diff.15 Gearbox, mechanics, gears, shafts, internal operation16 Final drive, differential, differential lock17 Front suspension, drive shafts18 Rear suspension, drive shaft19 Wheels, tyres. axle align20 ABS, ADR, TCS, EDL, ESP21 Brake, brake mechanics22 Brakes, hydraulics, regulator, servo23 Steering24 Body front25 Body centre, roof, frame26 Body, rear27 Bonnet, flaps, cab, central locking28 Front door, central locking29 Glazing/window mechanism30 Exterior equipment31 Interior equipment32 Passenger protection33 Trim, noise insulation34 Seat frames35 Seat padding, covers36 Heating37 Air conditioner38 Infotainment39 Windscreen wipe/wash system40 Lights, lamps, switches outside41 Lights, lamps, switches inside, anti-theft system42 Wiring
Skoda Citigo (NF, 2012 on)26 · Body, rear
26 · Body & interior

Part welding

Make
Skoda
Model
Citigo
Year
NF, 2012 on
Section
Replacing the lateral part › Part welding
Body, rearPart welding

Part welding

Replacing the lateral part · Citigo from 2012 · Edition 11.2011

Note

  • The new part must be welded within 90 minutes as otherwise the adhesion of the glue may be poor.
  • The threads for the locking clamp attachment must be cleaned from adhesive after glueing in.
  • 2K polyurethane adhesive D 180 KD2 A1 must be applied on the right lateral part, in the area of the tank filler neck, before welding.
N53-11458

Apply 2K epoxy adhesive DA 001 730 A2 in the areas shown.

Note

  • High and ultra high-strength and hot-formed steels are used in the area of the A, B and C-pillars. The welding bars in this area are approx. 16 mm wide.
  • If the welding points are positioned at the edge of the hot-formed panels, the structure of the plates is changed through the increase in temperature in such a way that it has a negative effect on the crash behaviour.
N51-12415

Therefore the welding points must be positioned as far as possible to the inside.

  • (a) of 8 mm can be obtained if the welding caps are chamfered.

Fit the new part on the vehicle standing on its wheels or on the straightening bracket set and fix.

Check the fit with component parts.

N53-11459

Weld lateral part, RP spot seam inverter.

Weld the separation cuts, optionally MIG L quilting seam / inert gas shielded full seam is permissible.

Note

  • Both welding symbols are shown in the illustration.

Weld the bonding on the bottom side rail, inert gas shielded plug weld.

Crimp the wheel arch strip.

Wipe off excess glue and seal wheel arch.

N53-11460

Weld the lateral part in the tailgate cutout, inert gas shielded plug weld.