Workshop Manuals Factory service & repair Skoda
01 Technical Data02 Self diagnosis, V.A.G Inspection Service03 Engine assy, cylinder block, crankcase04 Enginecrankshaft group, pistons05 Engine cylinder head, valve gear06 Engine lubrication07 Engine cooling08 Fuel supply, gas operation09 Mixture preparation system, electronic inj., Gas10 Exhaust system11 Starter-current supply-CC12 Ignition system, glow plug system13 Clutch, control14 Torque converter15 Gearbox mechanics, operation, construction, diff.16 Gearbox, mechanics, gears, shafts, internal operation17 Automatic gearbox, control, assembly, housing18 Automatic gearbox, gears, control19 Final drive, differential, differential lock20 Front suspension, drive shafts21 Rear suspension, drive shaft22 Wheels, tyres. axle align23 ABS, ADR, TCS, EDL, ESP24 Brake, brake mechanics25 Brakes, hydraulics, regulator, servo26 Steering27 Body front28 Body centre, roof, frame29 Body, rear30 Bonnet, flaps, cab, central locking31 Front door, central locking32 Exterior equipment33 Interior equipment34 Trim, noise insulation35 Seat padding, covers36 Air conditioner37 Infotainment38 Windscreen wipe/wash system39 Lights, lamps, switches outside40 Lights, lamps, switches inside, anti-theft system41 Wiring
Skoda Rapid (NA, 2011 on)28 · Body centre, roof, frame
28 · Body & interior

Part welding

Make
Skoda
Model
Rapid
Year
NA, 2011 on
Section
Replacing the outside bottom side rail › Part welding
Body centre, roof, framePart welding

Part welding

Replacing the outside bottom side rail · Rapid from 2011 · Edition 09.2011

Note

  • The new part must be welded within 90 minutes as otherwise the adhesion of the glue may be poor.
  • The holes for the hinge attachment must be cleaned from adhesive after glueing in.
N51-12160

Apply 2K epoxy adhesive DA 001 730 A2 in the areas shown.

Note

  • High and ultra high-strength and hot-formed steels are used in the area of the A, B and C-pillars. The welding bars in this area are approx. 13 mm wide.
  • If the welding points are positioned at the edge of the hot-formed panels, the structure of the plates is changed through the increase in temperature in such a way that it has a negative effect on the crash behaviour.
N51-12415

Therefore the welding points must be positioned as far as possible to the inside.

  • (a) of 8 mm can be obtained if the welding caps are chamfered.

Adjust the new part and fix. For this purpose, the vehicle is standing on its wheels or on the straightening bracket set.

Check the fit with component parts.

Note

  • (1), where welding is not permitted.
N51-12520

Weld the bottom side rail, RP spot seam inverter and inert gas shielded plug weld.

Weld the separation cuts, optionally MIG L soldered seams / inert gas shielded full seams are permissible.

Note

  • Both welding symbols are shown in the illustration.

Crimp the wheel arch flange.

Wipe off excess glue and seal wheel arch.

Parts & tools for this job For 2011 Skoda Rapid

As an Amazon Associate we earn from qualifying purchases.