Procedures for totally discharged batteries
- Make
- Volkswagen
- Model
- Caddy Mk3
- Year
- 2004–2015
- Section
- Battery › Procedures for totally discharged batteries
Procedures for totally discharged batteries
Note
- Heavily discharged batteries can freeze in winter due to the high water content in the electrolyte. If a battery is frozen it must not be charged. The reason for this is because the housing becomes defective in a frozen state.
Batteries that have not been used for a long time e.g. vehicles that have been stored, self-discharge.
On totally discharge batteries the electrolyte (sulphuric acid/water mixture) is almost all water, the sulphuric acid part is heavily reduced.
Totally discharged batteries sulphate, therefore all of the plate surfaces of the battery harden.
If a totally discharged battery is charged again shortly after it has lost its charge, the sulphation will dissipate.
If these batteries are not recharged the plates continue to harden and the ability to recharge is reduced. A reduction in the battery output is the result.
Totally discharge batteries must be charged with a small charging current as follows:
The charge current must be set at a maximum of 10 % of the battery capacity, therefore for a 60 Ah battery the charge current is a maximum 6A (ampere)
Charging battery → Chapter.
The charge period must be at least 24 hours.
Totally discharged batteries must never be charged quickly.
Parts & tools for this job For 2004 Volkswagen Caddy
- TOOLBattery testerSearch: car battery tester
- TOOLDigital multimeterSearch: automotive digital multimeter
- TOOLBattery terminal cleanerSearch: battery terminal cleaner
As an Amazon Associate we earn from qualifying purchases.